About 400 mV of voltage depression causes the camera to give up before using its full capacity
-
So I alternated covering and exposing the pan, which was likely a waste of my time
-
I like the wood-grain effect of the doubly curved recess
-
This is far below the level my cheap “instrumentation” can measure
-
The silicone molded over the LEDS turned out to be supremely un-stick-able to the tape
-
These black PETG-CF numbers seem plausible
-
The “aluminum oxide” curve shows 16% adsorption should correspond to more than 50% RH