This time I ignored boxes indicating humidity below 20%, because they’re doing fine.
Raw data for the other boxes:
| 2026-11-10 | ||||
| Filament | %RH | Weight – g | Wt gain – g | Gain % |
| TPU Clear | 26 | 53.3 | 3.3 | 6.6% |
| PETG-CF Blue | 23 | 53.2 | 3.2 | 6.4% |
| PETG Clear | 28 | 53.6 | 3.6 | 7.2% |
| 2026-11-17 | ||||
| Filament | %RH | Weight – g | Wt gain – g | Gain % |
| PETG Clear | 24 | 51.8 | 1.8 | 3.6% |
| 2026-11-20 | ||||
| Filament | %RH | Weight – g | Wt gain – g | Gain % |
| PETG Clear | 23 | 51.5 | 1.5 | 3.0% |
| TPU Clear | 22 | 52.0 | 2.0 | 4.0% |
| PETG-CF Blue | 26 | 53.2 | 3.2 | 6.4% |
What is becoming painfully obvious: 3D printer filament does not necessarily arrive bone-dry from the factory. Just-extruded nearly molten filament squirts out of the extruder and goes through several water baths for controlled cooling, after which it’s buffered in air, wound on spools, and vacuum-sealed with a little bitty packet of desiccant: Youtube will show you how that works.
For example, the nearly full PETG Clear filament spool I loaded in September has released nearly 15 g (!) of water vapor:
| PETG Clear | %RH | Weight – g | Wt gain – g | Gain % |
| 2026-09-07 | 37 | 54.4 | 4.4 | 8.8% |
| 2026-10-13 | 33 | 53.3 | 3.3 | 6.6% |
| 2026-11-10 | 28 | 53.6 | 3.6 | 7.2% |
| 2026-11-17 | 24 | 51.8 | 1.8 | 3.6% |
| 2026-11-21 | 23 | 51.5 | 1.5 | 3.0% |
| Total: | 14.6 |
Some water vapor certainly comes from the 50 %RH basement air filling the box while I change the desiccant, but Polydryer boxes with filament already at 10 %RH recover quickly.
Other than replacing desiccant on a regular basis, there doesn’t seem much else to do.
And, as always: Trust, but verify.